01314nam a2200301 c 4500001001300000005001500013008004100028040001100069041001300080052003000093245024000123300003200363545004700395545004700442545004700489545003700536653014200573700003600715700001400751700001400765700001900779773011800798856002000916900002000936900002000956900001700976900001900993KSI00006553620040112225121031118s1997 ulka 000 kor  a0110010 akorbeng01a559.705b한617ㅈc17(1)00aFe, Cr, Mn, Si, Ni의 첨가에 의한 고력황동의 미세조직과 마모특성=xMicrostructure and wear properties of high strength yellow brass by addition of Fe, Cr, Mn, Si and Ni/d박재용,e강춘식,e신윤호,e배정찬 ap. 258-266:b삽도;c26 cm a박재용, 서울대학교 금속공학과 a강춘식, 서울대학교 금속공학과 a신윤호, 서울대학교 금속공학과 a배정찬, 생산기술연구원 aFeaCraMnaSiaNia첨가a고력황동a미세조직a마모특성aMicrostructureaPropertiesaHighaStrengthaYellowaBrassaAddition1 a배정찬,d1954-0KAC2017220011 a강춘식1 a신윤호1 a박재용4aut0 t주조.d한국주조공학회.g17卷 3號(1997년 6월), p. 258-266q17:3<258w(011001)KSE199508743,x1017-451640u3047944aKd00010aBae, Jeong-Chan10aKang, Choon-Sik10aShin, Yun-Ho10aPark, Jae-Yong